How To Reduce The Loss After The Defect Of Precision Casting Parts?

In the production process of precision casting, due to the influence of many factors, there are often holes, pinholes, slag inclusion, cracks, pits and other defects. At this time, in order to make the castings meet the use standards and reduce the loss and waste, the casting foundry will often repair the defects. Commonly used repair equipment is argon arc welding machine, resistance welding machine, cold welding machine, etc.

_20221122163654

For casting defects that do not require high quality and appearance, argon arc welding machine and other welding machines with high heat and fast speed can be used to repair them. However, in the field of precision casting defect repair, due to the great influence of argon welding heat, casting deformation, hardness reduction, sand hole, local annealing, cracking, pinhole, wear, scratch, edge bite, or insufficient bonding force and internal stress damage and other secondary defects will be caused during repair.


Cold welding machine just overcome the above shortcomings, its advantages are mainly reflected in the small heat affected area, casting without preheating, cold welding repair at room temperature, so there is no deformation, edge bite and residual stress, no local annealing, do not change the metal structure of the casting. Therefore, cold welder is suitable for repairing surface defects of precision castings.


The welding repair range of cold welding is the process of repeated melting and accumulation of φ1.5-1.2 mm welding repair points. In the process of repairing large area defects, the repair efficiency is the factor restricting its widespread application. For major defects, the composite application of traditional welding repair process and casting defect repair machine is recommended. In the selection of cold welding machine, it is also necessary to choose the equipment with simple operation, high welding repair efficiency, high post-welding strength, post-welding shot blasting cleaning, mechanical processing without falling off and other advantages.


Choose such a cold welder, welding repair and grinding, completely can not see the repair marks. It is an important problem to satisfy the strength of the box parts under great stress. But for most boxes, the main index to evaluate the performance is stiffness, because the stiffness of the box not only affects the normal work of the transmission parts, but also affects the working accuracy of the parts. Fast and easy casting automatic selection is included.


The friction heating of the parts in the box changes the viscosity of lubricating oil and affects its lubrication performance; The temperature rise causes the thermal deformation of the box, especially the thermal deformation and thermal stress of the uneven distribution of temperature, which has a great influence on the accuracy and strength of the box. Such as the arrangement of fulcrum, reinforcement layout, opening position and connection structure design, are conducive to improving the strength and stiffness of the box.