Lost Wax Alluminum Casting

Lost Wax Alluminum Casting

Material: Aluminium Alloy
Process Investment casting(lost wax casting):
surface finishment: Ra1.6-Ra3.2
Size tolerance: VDG P690 D2
Maximum size: ≤1200mm×800mm×400mm
weight range: 0.1Kg-120Kg
Send Inquiry

Product Introduction

Description
This Lost Wax Alluminum Casting refers to the pure aluminum or aluminum alloy devices made by wax loss method. Its manufacturing process is generally to pour aluminum or aluminum alloy heated to liquid into sand mold or metal mold to obtain aluminum parts of various shapes and sizes. The product has high purification efficiency, long service life, low cost, easy installation and flexible use. It has some incomparable advantages over other castings, such as beauty, light weight, corrosion resistance, etc., which also makes it widely favored by users, especially in the automotive industry. The density of the product is smaller than that of cast iron and cast steel, while the specific strength is higher.

Features
The Lost Wax Alluminum Casting has good surface luster and good corrosion resistance in the atmosphere and fresh water, so it has a wide range of uses in the manufacture of civil utensils. Pure aluminum has good corrosion resistance in oxidizing acid media such as nitric acid and acetic acid, so aluminum castings have certain applications in chemical industry. Pure aluminum and aluminum alloys have good thermal conductivity and are often used as heat exchange materials in chemical production. This product has many advantages, making it one of the most popular casting products for customers. In the future, with the progress of aluminum alloy casting technology, it will show its style on a larger stage.


Chemical composition:

Si: 6.50-7.50

Mg: 0.25-0.45

Al: Blance

Fe: ≤0.50

Cu: ≤0.20

Mn: ≤0.35

Zn: ≤0.30

Ti+Zr: ≤0.25

Be: ≤0.10

SN: ≤0.01

Pb: ≤0.05


Physical property:

Tensile Strength: σb≥220MPa

Yield Strength: σ0.2≥180MPa

Extensibility: δ5 ≥2%

Hardness: 65-95HB


Specification of heat treatment:

Quenching---Rising the temperature to 535℃within 2H,keeping 8—12h,then cooling in 65℃ water,

Tempering--- Rising the temperature to 180±5℃within 1H,keeping 4~8h;then cooling in air.