Alloy Steel Lost Wax Casting

Alloy Steel Lost Wax Casting

Material: Alloy steel
Process Investment casting(lost wax casting):
surface finishment: Ra1.6-Ra3.2
Size tolerance: VDG P690 D2
Maximum size: ≤1200mm×800mm×400mm
weight range: 0.1Kg-120Kg
Send Inquiry

Product Introduction

Description

The Alloy Steel Lost Wax Casting is manufactured by wax loss casting method. The products cast with wax loss method have no traces of shell or gasket. It is better to cast hollowed out objects with it. China's traditional investment casting skills have a great impact on the international metallurgical development. The modern industrial investment precision casting is derived from the traditional wax loss method. Although they are quite different from each other in terms of wax materials, mold making, modeling materials and process methods, their process principles are the same.

 

Features
This Alloy Steel Lost Wax Casting is actually a medium carbon steel, cold heading die steel. This kind of steel is cheap and easy to process. After proper heat treatment, it has certain toughness, plasticity and wear resistance. Normalizing can promote the change of scoring organization and improve cutting performance. The alloy is tempered at 550~570 ℃, and its comprehensive mechanical properties are the best. This product has higher quenching degree than S45C steel, and is suitable for high frequency quenching and flame quenching.

 

Common materials:

CHINA

GB

USA

AISI

UK

BS

FRANCH

NF

GERMAN

DIN

JAPAN

JIS

40Cr

5140

530A40

42C4

41Cr4(1.7035)

SCr440

30CrMo

4130

/

30CD4

34CrMo4(1.7220)

SCM430

42CrMo

4140

708M40

42CD4

42CrMo4(1.7225)

SCM440

/

8620

805M20

0NCD2

/

SNCM220

 

Chemical composition:

C: ≤0.38-0.43

Si: ≤0.15-0.35

Mn: ≤0.70-0.90

P: ≤0.035

S: ≤0.040

Cr: 0.80-1.05

 

Physical property:

Tensile Strength: σb≥980 MPa

Yield Strength: σ0.2≥785 MPa

Extensibility: δ5 ≥9%

Hardness: ≤207HB

 

Specification of heat treatment:

Quenching at 850℃, oil colding; tempering at 520℃, water colding and oil colding. The surface hardness HRC 52-60, flame quenching can reaching HRC48-55.

Nitrogen treatment --- After QT and Nitrogen treatment, the maximum hardness can reaches HRC43~55.

 

Advanced Techniques:

Multi-layer ceramic shell system

Vacuum-assisted countergravity pouring

Computerized solidification control

HIP treatment available (100MPa/1120°C)

 

Quality Verification:

Spectrochemical analysis (OES)

Radiographic inspection (ASTM E94)

Ferrite content measurement

Salt spray testing (ASTM B117)