The mechanical properties of precision castings are higher than those of cast iron, but their casting properties are worse than those of cast iron. Because the melting point of stainless steel precision castings is high, the liquid steel is easy to oxidize, the fluidity of molten steel is poor, and the shrinkage is large, its volume shrinkage is 10 ~ 14%, and the linear shrinkage is 1.8 ~ 2.5%. In order to prevent the defects of steel castings such as insufficient pouring, cold shut, shrinkage cavity and porosity, crack and sand sticking, more complex process measures than cast iron must be taken:
Because the shrinkage of stainless steel precision castings is much higher than that of cast iron, in order to prevent shrinkage cavity and porosity defects, riser and, cold iron and subsidies are mostly used in the casting process to realize sequential solidification
Due to the poor fluidity of liquid steel, in order to prevent cold insulation and insufficient pouring of steel castings, the wall thickness of steel castings shall not be less than 8mm; The structure of the gating system of precision castings is as simple as possible, and the section size is larger than that of cast iron; Dry mold or hot mold shall be adopted;
Properly increase the pouring temperature, generally 1520 ° ~ 1600 ℃, because the pouring temperature is high, the superheat of molten steel is large, the liquid state is maintained for a long time, and the fluidity can be improved. However, if the pouring temperature is too high, it will cause defects such as coarse grains, hot cracks, pores and sand sticking. Therefore, the pouring temperature of small, thin-walled and complex castings is about the melting point temperature of steel + 150 ℃;
The pouring temperature of large and thick wall castings is about 100 ℃ higher than its melting point