The common defects in precision casting are bubbles, which refer to the lubrication hole defects in individual positions of fine castings. Bubbles are usually found after machining.
The common defects in precision casting are bubbles, which refer to the lubrication hole defects in individual positions of fine castings. Bubbles are usually found after machining. After years of workshop consumption experience, the technicians of Jibang precision casting summarized the causes and preventive measures of bubbles in precision casting as follows: 1. Composition reasons: 1. In most cases, bubbles are mainly due to insufficient roasting of the outer shell of fine casting, and a large amount of gas generated from the shell during molten steel pouring can not be discharged smoothly, which then intrudes into the liquid metal to form bubbles; 2. Due to the shell making process or shell mold data, the air permeability of the shell is too poor, and the gas in the cavity is difficult to be discharged, which enters the liquid metal to form bubbles; 3. The air drawn into the molten steel during pouring fails to be discharged, resulting in the formation of casting bubbles. 2、 Preventive measures 1. When the conditions of precision casting allow, set the exhaust bubble at the highest part of the casting with complex structure. 2. When designing the gating system, fully consider the shell exhaust demand. 3. The shell baking temperature and time shall be reasonable, and the holding time shall be sufficient. 4. During dewaxing, the wax material shall be thoroughly cleaned. 5. Properly reduce the interval from the ladle nozzle to the gate cup, and the pouring speed shall be average to ensure that the steel degree stably fills the mold cavity, and less air is involved in the molten steel as far as possible, so that the gas in the mold cavity and molten steel can be discharged smoothly.